whole CSF work for ass

Hello, I just broke over 1 week of work out of the door with ease! No matter if I have not sanded the paint, or sanded it or sanded it to the base -> everything could be broken out wonderfully. And indeed I have (tryed) the whole door interior sheet to dam with it or to seal it (the holes), so everything is futsch, tens of resin and mats, the door looks like a battlefield and my mood well. Whether I am at 25°C or at 18°C with 2%,1,5% Couldn’t they tell me that GFK doesn’t hold on to metal/lacquer?